Description
In cement concrete phenomenon of FSP-99 is observed as under:
- Even with 20% less water ensures homogeneous and consistant mortar mix with not risk of segregation.
- Due to fast wetting of cement lumps are formed and the cohesive mix insures compact mass formation thereby increasing strength of the concrete up to 20%.
- Increase workability and finish without raising cement water ratio. Reduces, cracks and shrinkage in cement concrete
- Early extra strength.
- It allows fast removal of form work due to early gain of strength with high mechanical properties
Doses:
(a) 200 gms. of FSP-99 is suffcient for 50 kg. of Portland cement which requires 8 days curing only and produces very dense water impermeable concrete.
(b) using 500 gms. of FSP-99 per 50kg. of Portland cement no curing is required, produces dense and water impermeable concrete within 8 days, resumes workable strength in 72 hours.





Reviews